Feller-Kniepmeier, Monika; Hemmersmeier, Ursula; Kuttner, Thomas; Link, Thomas. (1994). Analysis of Interfacial Dislocations in a Single Crystal Nickel-Base Superalloy After [001] Creep at 1033K: Evolution of Internal Stresses. Scripta Metallurgica et Materialia, Vol. 30, No. 10, S. 1275-1280.